V (TiCN)

V (TiCN)

V Coating


Composition: TiCN
GPa hardness: 35
Thickness: ~3 µm
Temp. Oxidation: 400 °C
Coefficient of Friction: 0.25
Features:
  • Wear resistance.
  • Slip wear resistance.
  • Optimal lubricity for threading process.
Processes:
  • Threading and Trimming Matrix.
Recommended Applications:
  • Threading.
  • Punching.
  • Milling.

Product inquiry and technical support